SAC305 Stick

Reference: SAC305
TECHNICAL DATA SHEET

Alloy SAC305

 Alloy S-Sn96.5 Ag3.5 Cu0.5

General Characteristics                                       

  • Ternary soldering alloy, lead free, used in the related electronic industry as well as in medical and food applications
  • The lowest melting point of the lead free alloys: 217°C
  • Very good mechanical strength
  • Shinning alloy, good capillarity
  • Satisfying electric conductance

Physico-Chimical Characteristics

  •  Tin rate “Sn”                            Rest
  • Copper rate « Cu »                    0.3 % à 0.6 %
  • Silver rate « Ag »                     3,0 % à 3,4 %
  • Melting temperature                 eutectic 217°C
  • Specific gravity                         7.3
  • Mechanical Strength                 Brinell hardness :14.8 H.B.
  • Electric conductance                 14% IACS
  • Electric resistance                     12.3 µ Ώ cm

QUALITY INSURANCE

Each delivery is identified by its manufacturing batch with the corresponding certificate of analysis

 Standard

International                             ISO 9453