SAC300 Solder Wire

TECHNICAL DATA SHEET

Alloy SAC300

 

Alloy S-Sn97-Ag3

General Characteristics                                          

Binary soldering alloy, lead free, used in the related electronic industry

Alloy whose melting range is 40°C higher than the alloy Sn63Pb37.

 

Physico-Chimical Characteristics

 Tin rate “Sn”                              Rest

Silver rate « Ag »                       3

Melting temperature                221°C-224°C

Specific gravity                          7.35

Mechanical Strength               Brinell hardness :15 H.B.

Electric conductance              14% IACS

Electric resistance                    12 µ cm

Iron soldering                              Minimum :  350 °C

Maximum : depending on flux

QUALITY INSURANCE

Each delivery is identified by its manufacturing batch with the corresponding certificate of analysis

 Standards

                   

International                             ISO 9453